| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black
Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT5100-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT5100-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black
Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade
Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural
Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black
Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products P254-00 Polypropylene Copolymer, Natural
Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural
Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products..
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black
Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade
Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black
Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 3.45 - 10.3 MPa | 500 - 1500 psi | |
|
BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant nylon 6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retard..
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural