| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products G13P100-589UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (YR169L) Mild Beige
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral
Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products P251-01 Polypropylene Copolymer, Black
Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products P256-01A Polypropylene Copolymer, Black
Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black
Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products T20P100-248 20% Talc Reinforced Polypropylene, General Purpose Grey
Applications: Durable goodsElectronics housingsHVAC ducts - air distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products T20P105-00FA 20% Talc Reinforced Polypropylene, FDA Compliant Components, Natural
Applications: Food traysFood service implementsContainersConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade
Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products M12P256-01 12% Mica Reinforced Polypropylene Copolymer, Black
Applications: Air damsAir ducts - distributionClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
|
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||