Polymer Property : Mold Temperature = 80.0 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black
Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black
Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products GC20P100-04 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, White
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White
Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products P102-00 Polypropylene, Black
Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products P250-01 Polypropylene Copolymer, Black
Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products P256-01A Polypropylene Copolymer, Black
Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated
Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade
Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 93.3 °C
80.0 - 200 °F
PTS Trimid® N66-G43HL 43% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 26.7 - 93.3 °C
80.0 - 200 °F
PTS Trimid® N66-T100 Toughened Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black
Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Styrolution Zylar 650 MBS
Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact..
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Ecomass® 720ZD91 Tungsten Filled ABS
High Specific GravityTungsten Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers
Mold Temperature 26.7 - 60.0 °C
80.0 - 140 °F
CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer
X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC).
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer
Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s..
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.