| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
Multibase Multi-Pro® 2516 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult..
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
Multibase Multi-Pro® 4518 CUW Polypropylene
Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal
Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P252-00 Polypropylene Copolymer, Natural
Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P256-01 Polypropylene Copolymer, Black
Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P257-00 Polypropylene Copolymer, Natural
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P257-01 Polypropylene Copolymer, Black
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black
Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P601-01 Polypropylene Copolymer, Black
Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black
Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
|
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t..
|
|||
| Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
|
LTL Color Compounds ColorFast® GPA100 ABS
High impact, high gloss injection molding ABS, HB-rated, FDAAll information provided by LTL Color Compounders, Inc.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||