Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hold Pressure = 8.27 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black
Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products GC30P103-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Battery traysFender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP514-01 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey
Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black
Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade
Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural
Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP514-00 14% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products HP522-473 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZU5A Dark Graphite
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 5.52 - 8.27 MPa
800 - 1200 psi
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Hold Pressure 2.07 - 8.27 MPa
300 - 1200 psi
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved