| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
Multibase Multi-Pro® 2516 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult..
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
Multibase Multi-Pro® 3019 CXUW Polypropylene
Calcium Carbonate Filler, 30% by weight.Features:Gloss, High Impact Resistance, GoodUV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn EquipmentInformation prov..
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P250-00 Polypropylene Copolymer, Natural
Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P252-01 Polypropylene Copolymer, Black
Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P254-00 Polypropylene Copolymer, Natural
Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P256-01A Polypropylene Copolymer, Black
Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P257-00 Polypropylene Copolymer, Natural
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black
Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products P601-01 Polypropylene Copolymer, Black
Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black
Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
|
Oxford Polymers ABS 20CCF-MP-BK ABS, 20% Carbon Fiber Reinforced
Conductive Carbon Fiber (20% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and extrusion/Injection Molding Additives: Release AgentsInformation provided by Oxford P..
|
|||
| Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
|
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
|
Star Plastics ABS5035 Molding Grade ABS
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have
an excellent soft t..
|
|||
| Rear Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9201-45 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Rear Barrel Temperature | 188 °C | 370 °F | |
|
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Rear Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
|
LTL Color Compounds ColorFast® GPA300X ABS
Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc.
|
|||
| Rear Barrel Temperature | 188 - 216 °C | 370 - 420 °F | |
|
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||