Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC10P200-01 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Black Applications: HousingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP521-501UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 149B Shale Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T20P100-01EG 20% Talc Reinforced Polypropylene, General Purpose Black, Extrusion Grade Applications: Consumer goodsAutomotive componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP516-01 7% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimCenter consolesHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 80.0 - 82.2 °C | 176 - 180 °F | Average value: 81.8 °C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
PolyOne Lubri-Tech™ AS-20GF/05T Acrylonitrile Butadiene Styrene (ABS), Glass Filled, PTFE Lubricated
(discont Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | Average value: 73.9 °C Grade Count:7 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 79.4 - 82.2 °C | 175 - 180 °F | Average value: 80.2 °C Grade Count:5 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |