| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige
Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products GC20P100-04 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, White
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products GC30P105-08FA 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black
Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral
Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP521-501UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 149B Shale
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products P102-00 Polypropylene, Black
Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products P252-01 Polypropylene Copolymer, Black
Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products P256-01 Polypropylene Copolymer, Black
Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products P256-01A Polypropylene Copolymer, Black
Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural
Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black
Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T20P100-248 20% Talc Reinforced Polypropylene, General Purpose Grey
Applications: Durable goodsElectronics housingsHVAC ducts - air distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural
Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade
Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide
Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black
Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
|
RheTech Products HP516-01 7% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trimCenter consolesHush panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Injection Pressure | 2.76 - 100 MPa | 400 - 14500 psi | Average value: 38.0 MPa Grade Count:5 |
|
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
|
|||
| Injection Pressure | 2.76 - 120 MPa | 400 - 17400 psi | Average value: 49.3 MPa Grade Count:44 |
|
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
|
|||