| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral
Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P104-00 Polypropylene, Natural
Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P107-00 Polypropylene Homopolymer, Natural
Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P252-00 Polypropylene Copolymer, Natural
Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P256-00 Polypropylene Copolymer, Natural
Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
|
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A..
|
|||
| Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
|
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV..
|
|||
| Nozzle Temperature | 182 - 216 °C | 360 - 421 °F | |
|
PolyOne Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where excepti..
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 188 - 216 °C | 370 - 420 °F | |
|
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer
Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for cons..
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC X-PRO CTC PP 3020 Polypropylene Copolymer
X-PRO PP 3020 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC X-PRO CTC PP 4025 Polypropylene Copolymer
X-PRO PP 4025 is a high value polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC X-PRO CTC PP 5002 Polypropylene Copolymer
X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer
X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC).
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC X-PRO PP 2021 Polypropylene Impact Copolymer
X-PRO PP 2021 is an impact, polypropylene copolymer. It has general purpose applications.Data provided by Composite Technologies (CTC).
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
|
CTC X-PRO PP 2050 Polypropylene Copolymer
X-PRO PP 2050 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
|
|||
| Nozzle Temperature | 199 - 216 °C | 390 - 420 °F | |
|
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
|
|||
| Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | Average value: 210 °C Grade Count:3 |
|
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..
|
|||