Polymer Property : Mold Temperature = 120 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products F22-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene, Black
Applications: Support ductsHousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White
Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade
Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products P252-01 Polypropylene Copolymer, Black
Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black
Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content
Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP 1097D Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP 1181 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP 1225 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-1580 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-1775D Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-1838-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2111S-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2137 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2250 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2320 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2634A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2750L1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2825E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2850E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2870UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-3004-HH Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP-2564A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
Mold Temperature 35.0 - 48.9 °C
95.0 - 120 °F
Teknor Apex Monprene® MP 1210A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..