| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT1004-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT2400-648UV Thermoplastic Polyolefin, UV Stabilized, 848 Black
Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products P100-00 Polypropylene, Natural
Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products P254-01 Polypropylene Copolymer, Black
Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products P257-01 Polypropylene Copolymer, Black
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black
Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
|
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced
Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
|
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
|
|||
| Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
|
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
|
|||
| Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
|
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol..
|
|||
| Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
|
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
|
|||
| Front Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t..
|
|||
| Front Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
|
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc..
|
|||
| Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
|
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||