| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.21 g/cc | 1.21 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 22 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
22 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength, Yield | 61.8 MPa <br>@Thickness 3.20 mm |
8960 psi <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | >= 150 % <br>@Thickness 3.20 mm |
>= 150 % <br>@Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 103 MPa <br>@Thickness 3.20 mm |
14900 psi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Flexural Modulus | 2.26 GPa <br>@Thickness 3.20 mm |
327 ksi <br>@Thickness 0.126 in |
10mm/min; ASTM D790 |
| Izod Impact, Notched | >= 6.86 J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C |
>= 12.9 ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | >= 130 °C <br>@Thickness 6.40 mm |
>= 266 °F <br>@Thickness 0.252 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 80.0 °C <br>@Thickness <=1.00 mm |
176 °F <br>@Thickness <=0.0394 in |
|
| 120 °C <br>@Thickness <=1.50 mm |
248 °F <br>@Thickness <=0.0591 in |
||
| 120 °C <br>@Thickness <=2.50 mm |
248 °F <br>@Thickness <=0.0984 in |
||
| 120 °C <br>@Thickness <=3.00 mm |
248 °F <br>@Thickness <=0.118 in |
||
| UL RTI, Mechanical with Impact | 80.0 °C <br>@Thickness >=1.00 mm |
176 °F <br>@Thickness >=0.0394 in |
|
| 110 °C <br>@Thickness >=1.50 mm |
230 °F <br>@Thickness >=0.0591 in |
||
| 110 °C <br>@Thickness >=2.50 mm |
230 °F <br>@Thickness >=0.0984 in |
||
| 110 °C <br>@Thickness >=3.00 mm |
230 °F <br>@Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 80.0 °C <br>@Thickness >=1.00 mm |
176 °F <br>@Thickness >=0.0394 in |
|
| 120 °C <br>@Thickness >=1.50 mm |
248 °F <br>@Thickness >=0.0591 in |
||
| 120 °C <br>@Thickness >=2.50 mm |
248 °F <br>@Thickness >=0.0984 in |
||
| 120 °C <br>@Thickness >=3.00 mm |
248 °F <br>@Thickness >=0.118 in |
||
| Flammability, UL94 | V-0 <br>@Thickness >=1.00 mm |
V-0 <br>@Thickness >=0.0394 in |
|
| V-0 <br>@Thickness >=1.50 mm |
V-0 <br>@Thickness >=0.0591 in |
||
| V-0 <br>@Thickness >=2.50 mm |
V-0 <br>@Thickness >=0.0984 in |
||
| V-0 <br>@Thickness >=3.00 mm |
V-0 <br>@Thickness >=0.118 in |
||
| 5VB <br>@Thickness >=2.50 mm |
5VB <br>@Thickness >=0.0984 in |
||
| 5VB <br>@Thickness >=3.00 mm |
5VB <br>@Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | |
| Hot Wire Ignition, HWI | 15 - 30 sec <br>@Thickness >=1.50 mm |
15 - 30 sec <br>@Thickness >=0.0591 in |
|
| 30 - 60 sec <br>@Thickness >=3.00 mm |
30 - 60 sec <br>@Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | >= 120 arcs <br>@Thickness 1.50 mm |
>= 120 arcs <br>@Thickness 0.0591 in |
|
| >= 120 arcs <br>@Thickness 3.00 mm |
>= 120 arcs <br>@Thickness 0.118 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
| Middle Barrel Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
| Front Barrel Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
| Nozzle Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
| Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
| Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | Injection Molding |
| Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
| Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
| Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |