Processing Properties Metric English Comments
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical LUCEL N127-AS Antistatic POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
Injection Molding
LG Chemical LUCON 6080EX ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio..
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance
Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information ..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY GP2102 PC+GF10%
Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance
Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature
Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY SC1004AU PC, High Impact
Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY SC2302 PC+GF30%, High Impact
Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY SR3108L PC, High Impact
Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical
Back Pressure 0.490 - 3.92 MPa
71.1 - 569 psi
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Back Pressure 0.490 - 3.92 MPa
71.1 - 569 psi
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Back Pressure 0.490 - 3.92 MPa
71.1 - 569 psi
LG Chemical LUPOL HM-5204B High Modulus Polypropylene, 20% Polymer Alloy, High Strength, High Flow, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Back Pressure 0.490 - 3.92 MPa
71.1 - 569 psi
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY GP1000MU PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C..
Back Pressure 1.96 - 3.92 MPa
284 - 569 psi
Injection Molding
LG Chemical XR407D ABS
Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical
Back Pressure 1.96 - 3.92 MPa
284 - 569 psi
Injection Molding
LG Chemical XR407E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by..
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance
Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..