Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 500R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 923 PC Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 923ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific) Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 950 PC Opaque colors, high viscosity, superior flame retardance. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten, PLC code 7; ASTM D 495 |
SABIC Innovative Plastics Lexan® 955U PC Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm). |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 925 PC Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 925A PC Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 925AU PC Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 945A PC Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D492 |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific) Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 2312 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL PX1543 PPE+PS |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® FL1000 PC 5% GR. Various weight reductions at .250""(6.35mm) wall. Excellent flex strength/rigidity, high heat/creep resistance. V-0/5VA rated. |