Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow
Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow
Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 3.00 mm
176 °F

@Thickness 0.118 in
UL 746
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow
Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 3.00 mm
176 °F

@Thickness 0.118 in
UL 746
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 3.00 mm
176 °F

@Thickness 0.118 in
UL 746
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1302-07 Polycarbonate Resin
Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=2.50 mm
176 °F

@Thickness >=0.0984 in
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by ..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=3.00 mm
176 °F

@Thickness >=0.118 in
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by ..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information ..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=3.00 mm
176 °F

@Thickness >=0.118 in
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information ..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY HI1002ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=3.00 mm
176 °F

@Thickness >=0.118 in
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=1.70 mm
176 °F

@Thickness >=0.0669 in
LG Chemical LUPOY SC3154 PC+GF15%
Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=0.850 mm
176 °F

@Thickness >=0.0335 in
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin
Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=1.00 mm
176 °F

@Thickness >=0.0394 in
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=3.20 mm
176 °F

@Thickness >=0.126 in
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=1.00 mm
176 °F

@Thickness >=0.0394 in
LG Chemical LUPOY GP1006FL PC, Flame Retardant
Description: Injection Molding, PC, Flame Retardant, High FlowApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.889 mm
176 °F

@Thickness 0.0350 in
UL 746
Teknor Apex APEX® 1015 Polyvinyl Chloride, Semi-Rigid
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.889 mm
176 °F

@Thickness 0.0350 in
UL 746
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.889 mm
176 °F

@Thickness 0.0350 in
UL 746
Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 1.40 mm
176 °F

@Thickness 0.0551 in
UL 746
Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
UL RTI, Mechanical without Impact 80.0 °C

@Thickness 0.889 mm
176 °F

@Thickness 0.0350 in
UL 746
Teknor Apex APEX® 1013 Polyvinyl Chloride, Semi-Rigid
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded ..