Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical with Impact = 80.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 3.00 mm
176 °F

@Thickness 0.118 in
UL 746
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.70 mm
176 °F

@Thickness 0.0669 in
UL 746
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced
Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow
Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow
Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release
Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release
Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release
Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.749 mm
176 °F

@Thickness 0.0295 in
UL 746
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow
Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer  (Unverified Data**)
Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 3.00 mm
176 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer  (Unverified Data**)
Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=2.50 mm
176 °F

@Thickness >=0.0984 in
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by ..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=3.00 mm
176 °F

@Thickness >=0.118 in
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY HI1002ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin
Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=1.50 mm
176 °F

@Thickness >=0.0591 in
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=2.50 mm
176 °F

@Thickness >=0.0984 in
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=2.00 mm
176 °F

@Thickness >=0.0787 in
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 3.00 mm
176 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.500 mm
176 °F

@Thickness >=0.0197 in
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin
Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Copyright © lookpolymers.com All Rights Reserved