Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
PolyOne OnForce™ LFT AM-30LCF/001 Grey Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
PolyOne OnForce™ LFT NN-30LCF/002 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
PolyOne OnForce™ LFT NN-50LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 270 - 320 °C | 518 - 608 °F | |
PolyOne Edgetek® QT-30GF/000 Natural Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Melt Temperature | 275 - 320 °C | 527 - 608 °F | |
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Melt Temperature | 275 - 320 °C | 527 - 608 °F | |
LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Polycarbonate (PC). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Melt Temperature | 260 - 320 °C | 500 - 608 °F | Die Melt Temp |
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating LDPE LA 0710 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum. High draw down, low neck in.In.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 2806 Polycarbonate ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 3107 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minGeneral purposeHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpare.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® LQ3187 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Dry, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® LED2245 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |