| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 1.70 mm
|
176
°F <br>@Thickness 0.0669 in
|
UL 746 |
|
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced
Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 3.00 mm
|
176
°F <br>@Thickness 0.118 in
|
UL 746 |
|
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced
Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 0.749 mm
|
176
°F <br>@Thickness 0.0295 in
|
UL 746 |
|
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow
Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 3.00 mm
|
176
°F <br>@Thickness 0.118 in
|
UL 746 |
|
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release
Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 1.50 mm
|
176
°F <br>@Thickness 0.0591 in
|
UL 746 |
|
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 3.00 mm
|
176
°F <br>@Thickness 0.118 in
|
UL 746 |
|
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 1.50 mm
|
176
°F <br>@Thickness 0.0591 in
|
UL 746B |
|
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer
(Unverified Data**)
Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=3.00 mm
|
176
°F <br>@Thickness >=0.118 in
|
|
|
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information ..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=1.50 mm
|
176
°F <br>@Thickness >=0.0591 in
|
|
|
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=3.00 mm
|
176
°F <br>@Thickness >=0.118 in
|
|
|
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=2.50 mm
|
176
°F <br>@Thickness >=0.0984 in
|
|
|
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=1.50 mm
|
176
°F <br>@Thickness >=0.0591 in
|
|
|
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=3.00 mm
|
176
°F <br>@Thickness >=0.118 in
|
|
|
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=3.00 mm
|
176
°F <br>@Thickness >=0.118 in
|
|
|
LG Chemical LUPOY HI1002ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.750 mm
|
176
°F <br>@Thickness >=0.0295 in
|
|
|
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=1.70 mm
|
176
°F <br>@Thickness >=0.0669 in
|
|
|
LG Chemical LUPOY SC3154 PC+GF15%
Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.850 mm
|
176
°F <br>@Thickness >=0.0335 in
|
|
|
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.850 mm
|
176
°F <br>@Thickness >=0.0335 in
|
|
|
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.500 mm
|
176
°F <br>@Thickness >=0.0197 in
|
|
|
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.500 mm
|
176
°F <br>@Thickness >=0.0197 in
|
|
|
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin
Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.500 mm
|
176
°F <br>@Thickness >=0.0197 in
|
|
|
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.500 mm
|
176
°F <br>@Thickness >=0.0197 in
|
|
|
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=1.00 mm
|
176
°F <br>@Thickness >=0.0394 in
|
|
|
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=3.00 mm
|
176
°F <br>@Thickness >=0.118 in
|
|
|
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=3.00 mm
|
176
°F <br>@Thickness >=0.118 in
|
|
|
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Impact, Chemical ResistanceApplication: IT/OA (M/P Battery Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information prov..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=1.60 mm
|
176
°F <br>@Thickness >=0.0630 in
|
|
|
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=3.20 mm
|
176
°F <br>@Thickness >=0.126 in
|
|
|
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=2.50 mm
|
176
°F <br>@Thickness >=0.0984 in
|
|
|
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness 1.50 mm
|
176
°F <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
|
|||
| UL RTI, Mechanical with Impact |
80.0
°C <br>@Thickness >=0.500 mm
|
176
°F <br>@Thickness >=0.0197 in
|
|
|
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin
Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
|
|||