Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | |
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | |
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUCON CP6080LP PC+CNT+GF Description: Injection Molding, PC+CNT+GF, Electrostatic Dissipation, Low Surface TribochargeApplication: ATM parts, HDD BracketCAS No. 103598-77-2, 65997-17-3 and 7782-42-5Information provided by L.. |
|||
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | Injection Molding |
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | |
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | Injection Molding |
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | Injection Molding |
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | |
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | |
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
Front Barrel Temperature | 290 - 305 °C | 554 - 581 °F | Injection Molding |
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | |
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced Vyteen PCGF10BK is a 10% fiberglass reinforced general purpose Polycarbonate grade.Features: - Good processabilityTypical Applications: - Laptop computer docking - Laser printer gear - Toner car.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant Feature: Injection Molding, sPS+GF30%, Flame RetardantApplication: Pump Units, Pick-up Lends Holder, etcCAS No. 9003-53-6, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 290 °C | 554 °F | |
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Front Barrel Temperature | 290 - 295 °C | 554 - 563 °F | |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion Coating |
DuPont Nucrel® 30907 Ethylene Acid Copolymer Resin Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The.. |
|||
Front Barrel Temperature | 290 °C | 554 °F | |
Beijing Chemical Industry KAIFA® M109-G20 MPPO Resin 20% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 290 - 330 °C | 554 - 626 °F | Injection Molding |
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Front Barrel Temperature | 290 °C | 554 °F | Extrusion lamination |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Front Barrel Temperature | 290 - 310 °C | 554 - 590 °F | Injection Molding |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |