| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 6.40 mm
|
493
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | ISO 75/Bf |
|
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY
Description: High flow Polyamide PA66 Flame retarded grade reinforced with 30% glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applicat..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66
LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA
LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66
LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific)
LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF002SXS PA 66
LNP* THERMOCOMP* RF002SXS is a compound based on Nylon 66 resin contaning 10% Glass Fiber. Characteristcs of this grade are: Heat Stabilized.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66
LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66
LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF003H PA 66
LNP* THERMOCOMP* RF003H is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF003XXH PA 66
LNP* THERMOCOMP* RF003XXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this grade is: Healthcare.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66
LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for ..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66
LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66
LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
|
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66
LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66
LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA
30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP STAT-KON RE0029 PA 66
LNP* STAT-KON* RE0029 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOTUF VF004S PA 66
LNP THERMOTUF* VF004S is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP VERTON RVL28 PA 66
LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | ISO 75-1/-2 |
|
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Information provided by Unitika Ltd.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | ISO 75 |
|
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant
Impact modified, 13% glass fiber reinforced, heat resistant Nylon 66 for injection molding applications.Information provided by Polyram.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | DAM; ISO 75-1/-2 |
|
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
|
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
|
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
|
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | ISO 75 |
|
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.
|
|||
| Deflection Temperature at 0.46 MPa (66 psi) |
256
°C <br>@Thickness 3.20 mm
|
493
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.
|
|||