| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.40 g/cc | 0.0506 lb/in³ | |
| 1.60 g/cc | 0.0578 lb/in³ | DAM; ISO 1183 | |
| Moisture Absorption | 0.700 % <br>@Thickness 2.00 mm |
0.700 % <br>@Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity | 79440 cP <br>@Shear Rate 5000 1/s,<br> Temperature 280 °C |
79440 cP <br>@Shear Rate 5000 1/s,<br> Temperature 536 °F |
ISO 11403-1 -2 |
| 101000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 270 °C |
101000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 518 °F |
ISO 11403-1 -2 | |
| 131520 cP <br>@Shear Rate 5000 1/s,<br> Temperature 260 °C |
131520 cP <br>@Shear Rate 5000 1/s,<br> Temperature 500 °F |
ISO 11403-1 -2 | |
| 259970 cP <br>@Shear Rate 500 1/s,<br> Temperature 280 °C |
259970 cP <br>@Shear Rate 500 1/s,<br> Temperature 536 °F |
ISO 11403-1 -2 | |
| 350400 cP <br>@Shear Rate 500 1/s,<br> Temperature 270 °C |
350400 cP <br>@Shear Rate 500 1/s,<br> Temperature 518 °F |
ISO 11403-1 -2 | |
| 474700 cP <br>@Shear Rate 500 1/s,<br> Temperature 260 °C |
474700 cP <br>@Shear Rate 500 1/s,<br> Temperature 500 °F |
ISO 11403-1 -2 | |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 170 MPa | 24700 psi | DAM; ISO 527-1/-2 |
| Tensile Stress | 3.79 MPa <br>@Strain 0.100 %,<br> Temperature 150 °C |
550 psi <br>@Strain 0.100 %,<br> Temperature 302 °F |
DAM; ISO 11403-1 -2 |
| 8.28 MPa <br>@Strain 0.100 %,<br> Temperature -40.0 °C |
1200 psi <br>@Strain 0.100 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 9.09 MPa <br>@Strain 0.100 %,<br> Temperature 23.0 °C |
1320 psi <br>@Strain 0.100 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 32.28 MPa <br>@Strain 0.400 %,<br> Temperature -40.0 °C |
4682 psi <br>@Strain 0.400 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 32.69 MPa <br>@Strain 0.700 %,<br> Temperature 150 °C |
4741 psi <br>@Strain 0.700 %,<br> Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 34.85 MPa <br>@Strain 0.400 %,<br> Temperature 23.0 °C |
5055 psi <br>@Strain 0.400 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 47.98 MPa <br>@Strain 1.30 %,<br> Temperature 150 °C |
6959 psi <br>@Strain 1.30 %,<br> Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 57.17 MPa <br>@Strain 1.90 %,<br> Temperature 150 °C |
8292 psi <br>@Strain 1.90 %,<br> Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 61.31 MPa <br>@Strain 0.700 %,<br> Temperature -40.0 °C |
8892 psi <br>@Strain 0.700 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 63.02 MPa <br>@Strain 0.700 %,<br> Temperature 23.0 °C |
9140 psi <br>@Strain 0.700 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 68.67 MPa <br>@Strain 3.70 %,<br> Temperature 150 °C |
9960 psi <br>@Strain 3.70 %,<br> Temperature 302 °F |
DAM; ISO 11403-1 -2 | |
| 87.65 MPa <br>@Strain 1.00 %,<br> Temperature 23.0 °C |
12710 psi <br>@Strain 1.00 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 88.75 MPa <br>@Strain 1.00 %,<br> Temperature -40.0 °C |
12870 psi <br>@Strain 1.00 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 141.41 MPa <br>@Strain 2.00 %,<br> Temperature 23.0 °C |
20510 psi <br>@Strain 2.00 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 186.16 MPa <br>@Strain 2.60 %,<br> Temperature -40.0 °C |
27000 psi <br>@Strain 2.60 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| Elongation at Break | 2.5 % | 2.5 % | DAM; ISO 527-1/-2 |
| Tensile Modulus | 7.50 GPa | 1090 ksi | 50%RH; ISO 527-1/-2 |
| 10.64 GPa | 1543 ksi | DAM; ISO 527-1/-2 | |
| Flexural Modulus | 9.45 GPa | 1370 ksi | DAM; ISO 178 |
| Secant Modulus | 2.77 GPa <br>@Strain 2.90 %,<br> Temperature 100 °C |
402 ksi <br>@Strain 2.90 %,<br> Temperature 212 °F |
DAM; ISO 11403-1 -2 |
| 3.45 GPa <br>@Strain 2.10 %,<br> Temperature 100 °C |
500 ksi <br>@Strain 2.10 %,<br> Temperature 212 °F |
DAM; ISO 11403-1 -2 | |
| 4.35 GPa <br>@Strain 1.30 %,<br> Temperature 100 °C |
631 ksi <br>@Strain 1.30 %,<br> Temperature 212 °F |
DAM; ISO 11403-1 -2 | |
| 5.892 GPa <br>@Strain 0.500 %,<br> Temperature 100 °C |
854.6 ksi <br>@Strain 0.500 %,<br> Temperature 212 °F |
DAM; ISO 11403-1 -2 | |
| 6.60 GPa <br>@Strain 0.100 %,<br> Temperature 100 °C |
957 ksi <br>@Strain 0.100 %,<br> Temperature 212 °F |
DAM; ISO 11403-1 -2 | |
| 7.80 GPa <br>@Strain 1.60 %,<br> Temperature 23.0 °C |
1130 ksi <br>@Strain 1.60 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 7.9245 GPa <br>@Strain 2.00 %,<br> Temperature -40.0 °C |
1149.4 ksi <br>@Strain 2.00 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 8.07 GPa <br>@Strain 0.400 %,<br> Temperature -40.0 °C |
1170 ksi <br>@Strain 0.400 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 8.28 GPa <br>@Strain 0.100 %,<br> Temperature -40.0 °C |
1200 ksi <br>@Strain 0.100 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 8.46 GPa <br>@Strain 1.20 %,<br> Temperature 23.0 °C |
1230 ksi <br>@Strain 1.20 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 8.7125 GPa <br>@Strain 0.400 %,<br> Temperature 23.0 °C |
1263.7 ksi <br>@Strain 0.400 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 8.81 GPa <br>@Strain 1.20 %,<br> Temperature -40.0 °C |
1280 ksi <br>@Strain 1.20 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 8.84 GPa <br>@Strain 0.800 %,<br> Temperature -40.0 °C |
1280 ksi <br>@Strain 0.800 %,<br> Temperature -40.0 °F |
DAM; ISO 11403-1 -2 | |
| 8.975 GPa <br>@Strain 0.800 %,<br> Temperature 23.0 °C |
1302 ksi <br>@Strain 0.800 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| 9.09 GPa <br>@Strain 0.100 %,<br> Temperature 23.0 °C |
1320 ksi <br>@Strain 0.100 %,<br> Temperature 73.4 °F |
DAM; ISO 11403-1 -2 | |
| Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | DAM; ISO 179/1eU |
| Charpy Impact, Notched | 1.13 J/cm² | 5.38 ft-lb/in² | DAM; ISO 179/1eA |
| 1.08 J/cm² <br>@Temperature -40.0 °C |
5.14 ft-lb/in² <br>@Temperature -40.0 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 19.0 µm/m-°C | 10.6 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | DAM; ISO 11359-1/-2 |
| Specific Heat Capacity | 1.66 J/g-°C | 0.397 BTU/lb-°F | |
| Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | of melt |
| Melting Point | 261 °C | 502 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 256 °C | 493 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 246 °C | 475 °F | DAM; ISO 75-1/-2 |
| Glass Transition Temp, Tg | 80.0 °C | 176 °F | DAM; 10°C/min; DS; ISO 11357-1/-2 |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
| V-0 <br>@Thickness 0.300 mm |
V-0 <br>@Thickness 0.0118 in |
DAM; IEC 60695-11-10 | |
| 5VA <br>@Thickness 1.50 mm |
5VA <br>@Thickness 0.0591 in |
DAM; IEC 60695-11-20 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | DAM; IEC 60093 |
| Dielectric Strength | 38.0 kV/mm | 965 kV/in | DAM; IEC 60243-1 |
| Dissipation Factor | 0.018 <br>@Frequency 100 Hz |
0.018 <br>@Frequency 100 Hz |
DAM; IEC 60250 |
| 0.018 <br>@Frequency 1.00e+6 Hz |
0.018 <br>@Frequency 1.00e+6 Hz |
DAM; IEC 60250 | |
| Comparative Tracking Index | 285 V | 285 V | DAM; IEC 60112 |
| 250 - 400 V | 250 - 400 V | DAM; UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additives | Release agent | |
| Delivery Form | Pellets |