| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP LUBRICOMP |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.250 % | 0.250 % | 50% RH, 24 hrs; ASTM D570 |
| 0.410 % | 0.410 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.010 - 0.030 cm/cm @Time 86400 sec |
0.010 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 101 MPa | 14600 psi | Type I, 5 mm/min; ASTM D638 |
| 104 MPa | 15100 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 111 MPa | 16100 psi | Type I, 5 mm/min; ASTM D638 |
| Elongation at Break | 1.5 % | 1.5 % | 5 mm/min; ISO 527 |
| 1.8 % | 1.8 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 9.37 GPa | 1360 ksi | 1 mm/min; ISO 527 |
| 9.85 GPa | 1430 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 154 MPa | 22300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 155 MPa | 22500 psi | ISO 178 | |
| Flexural Modulus | 8.36 GPa | 1210 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 8.49 GPa | 1230 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 4.00 J @Temperature 23.0 °C |
2.95 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.45 | 0.45 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.48 | 0.48 | ASTM D3702 Modified |
| K (wear) Factor | 6.04 x 10<sup>-8</sup> mm³/N-M | 3.00 x 10<sup>-10</sup> in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
| 64.5 x 10<sup>-8</sup> mm³/N-M | 32.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 63.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C | 491 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 256 °C @Thickness 3.20 mm |
493 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 232 °C | 450 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 239 °C @Thickness 3.20 mm |
462 °F @Thickness 0.126 in |
unannealed; ASTM D648 |