Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vyncolit 2530 W Novolac Phenolic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit 2530 W Novolac Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Powder Density; ISO 60
Density 1.58 g/cc
0.0571 lb/in³
Relative Density; ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 - 50.0 MPa
5800 - 7250 psi
ISO 527
Elongation at Break 0.55 - 0.65 %
0.55 - 0.65 %
Tensile; ISO 527
1.2 - 1.4 %
1.2 - 1.4 %
Flexure; ISO 178
Tensile Modulus 9.00 - 11.0 GPa
1310 - 1600 ksi
ISO 527
Flexural Strength 80.0 - 100 MPa
11600 - 14500 psi
At Rupture; ISO 178
Flexural Modulus 6.50 - 8.00 GPa
943 - 1160 ksi
ISO 178
Compressive Strength 200 - 230 MPa
29000 - 33400 psi
ISO 604
Charpy Impact Unnotched 0.600 - 0.800 J/cm²
2.86 - 3.81 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.200 - 0.300 J/cm²
0.952 - 1.43 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 - 40.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 22.2 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 160 - 180 °C
320 - 356 °F
ISO 75 Af
Deflection Temperature at 8.0 MPa 130 - 150 °C
266 - 302 °F
ISO 75 C
Flammability, UL94 V-1

@Thickness 1.60 mm
V-1

@Thickness 0.0630 in
V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
Shrinkage 0.15 - 0.30 %
0.15 - 0.30 %
Post Shrinkage; ISO 2577
Electrical Properties Metric English Comments
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 243
Comparative Tracking Index 175 V
175 V
IEC 112
Descriptive Properties Value Comments
Color Black
ISO type PF 2 C3
Main Filler Mineral & Organic
Molding Method Compression, transfer, injection
Users viewing this material also viewed the following: