Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Nabaltec ACTILOX® B20 AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Nabaltec APYMAG® 30S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 155 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 155 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and go.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
Total Finaprene® 602D Clear Impact Polystyrene
(discontinued **) Finaprene® 602D is a clear high styrenic styrene-butadiene (SBS) block copolymer with a radial structure, which is widely used as modifiers or in alloys with many plastic resins, such polystyrene, .. |
|||
Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Magyar Aluminum ALO-P54-04 Alumina Alumina for Polishing |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | DIN-53466 |
Iran Petrochemical (PCC) PVC-S6558 Poly Vinyl Chloride Grade S6558 has low porosity & high bulk density.Applications: pipe and fitting, injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Silon TA 2343 HD Black Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD, TA 1116 HD and TA 1117 HD.TA 2343 HD, together with the above mentioned graft, contains the cross-linking catalyst to.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | Size D (apparent) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 1183 |
Polyram RamClean™ 101 Purging Agent Purging agent for injection molding machines.Information provided by Polyram. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 186 PVC PVC Copolymer Suspension Resin F-186 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-186 .. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Axion Polymers Axplas® PS04 0000 Mixed Polystyrene Granules with FR The PS04 series of clean, mixed polystyrene granular chips offers a low-cost option for manufacturers to add post-consumer, engineering polymers to a wide range of products. The polymer mix includes.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Neopor® 5300 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® F 215 T-N Expandable Polystyrene Use: Expanding-agent containing plastic for the production of foam plasticInformation provided by BASF |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Peripor® 300 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® P 326 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 172 PVC PVC Copolymer Suspension Resin F-172 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-172 .. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Neopor® 2400 CT Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 7579 Phenolic, Granular, Compression Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 100 General Purpose Polystyrene for Injection Molding Product Description: General purpose Polystyrene PS 100 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with good flow properti.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |