Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 20.0 - 40.0 µm/m-°C @Temperature 50.0 - 150 °C |
11.1 - 22.2 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
CTE, linear, Parallel to Flow | 35.0 - 40.0 µm/m-°C @Temperature 50.0 - 150 °C |
19.4 - 22.2 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
CTE, linear, Parallel to Flow | 10.0 - 40.0 µm/m-°C @Temperature 50.0 - 150 °C |
5.56 - 22.2 µin/in-°F @Temperature 122 - 302 °F |
Post shrinkage; ISO 11359-2 |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 40.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 22.2 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 40.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 22.2 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 40.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 22.2 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
CTE, linear, Parallel to Flow | 35.0 - 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4 - 22.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
CTE, linear, Parallel to Flow | 35.0 - 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4 - 22.2 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
CTE, linear, Parallel to Flow | 35.0 - 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4 - 22.2 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
CTE, linear, Parallel to Flow | 30.0 - 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 22.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |