Polymer Property : Charpy Impact Unnotched = 3.81 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.600 - 0.800 J/cm²

@Temperature 23.0 °C
2.86 - 3.81 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eU
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Charpy Impact Unnotched 0.500 - 0.800 J/cm²
2.38 - 3.81 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Charpy Impact Unnotched 0.600 - 0.800 J/cm²
2.86 - 3.81 ft-lb/in²
ISO 179
Vyncolit 2530 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba..
Charpy Impact Unnotched 0.650 - 0.800 J/cm²
3.09 - 3.81 ft-lb/in²
ISO 179
Vyncolit 2920 W Novolac Phenolic
Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B..
Charpy Impact Unnotched 0.600 - 0.800 J/cm²
2.86 - 3.81 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RESINOL® 400 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Charpy Impact Unnotched 0.650 - 0.800 J/cm²

@Temperature 23.0 °C
3.09 - 3.81 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group 5557 DAP  (discontinued **)
Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h..
Charpy Impact Unnotched 0.800 - 0.800 J/cm²

@Temperature -20.0 - -20.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.800 J/cm² Grade Count:1
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..