Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² @Temperature 23.0 °C |
2.86 - 3.81 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Charpy Impact Unnotched | 0.600 - 1.70 J/cm² | 2.86 - 8.09 ft-lb/in² | Average value: 1.12 J/cm² Grade Count:5 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 0.600 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
2.86 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.813 J/cm² Grade Count:19 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact Unnotched | 0.600 - 1.36 J/cm² | 2.86 - 6.47 ft-lb/in² | Average value: 0.889 J/cm² Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage
(discontinued **)& Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bak AGBak AG became a pa.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² - NB @Temperature -30.0 - -30.0 °C |
2.86 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 4.09 J/cm² Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² | 2.86 ft-lb/in² | |
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² | 2.86 - 3.81 ft-lb/in² | ISO 179 |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9373 High-Heat Polycarbonate Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Charpy Impact Unnotched | >= 0.600 J/cm² | >= 2.86 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe PF CC 204 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts.Information provided by Hippe. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnitel® UM552 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, Dry as Molded
(discontinued **) Injection molding grade, higher stiffness, good stress corrosion cracking resistance and chemical resistance (fuel, cleaning agents).Information provided by Bayer.LANXESS was spun-off from Bayer in .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² - NB @Temperature -30.0 - -30.0 °C |
2.86 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 0.600 J/cm² Grade Count:3 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | >= 0.600 J/cm² @Temperature 23.0 °C |
>= 2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 0.600 - 0.800 J/cm² | 2.86 - 3.81 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² | 2.86 ft-lb/in² | |
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnitel® UM551 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact Unnotched | 0.600 - 1000 J/cm² | 2.86 - 4760 ft-lb/in² | Average value: 3.37 J/cm² Grade Count:13 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact Unnotched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |