Price EMAIL US    sales@lookpolymers.com
Material Notes:
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional stability. Xenoy X4810 resin can be considered for body panels, safety equipment, housings, doorhandles, spring-loaded applications, medical device enclosures, outdoor sports equipment.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Moisture Absorption 0.140 %
0.140 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.42 %
0.42 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
<br>@Thickness 3.20 mm
0.0070 - 0.0090 in/in
<br>@Thickness 0.126 in
SABIC Method
Melt Flow 12 g/10 min
<br>@Load 5.00 kg,<br> Temperature 266 °C
12 g/10 min
<br>@Load 11.0 lb,<br> Temperature 511 °F
ASTM D1238
Melt Index of Compound 10 g/10 min
<br>@Load 5.00 kg,<br> Temperature 265 °C
10 g/10 min
<br>@Load 11.0 lb,<br> Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
Tensile Strength at Break 55.0 MPa
7980 psi
5 mm/min; ISO 527
55.0 MPa
7980 psi
50 mm/min; ISO 527
60.0 MPa
8700 psi
Type I, 50 mm/min; ASTM D638
65.0 MPa
9430 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa
7980 psi
Type I, 5 mm/min; ASTM D638
55.0 MPa
7980 psi
5 mm/min; ISO 527
58.0 MPa
8410 psi
Type I, 50 mm/min; ASTM D638
60.0 MPa
8700 psi
50 mm/min; ISO 527
Elongation at Break 100 %
100 %
5 mm/min; ISO 527
100 %
100 %
50 mm/min; ISO 527
150 %
150 %
Type I, 50 mm/min; ASTM D638
150 %
150 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 4.1 %
4.1 %
5 mm/min; ISO 527
4.1 %
4.1 %
50 mm/min; ISO 527
4.5 %
4.5 %
Type I, 50 mm/min; ASTM D638
4.7 %
4.7 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 2.75 GPa
399 ksi
1 mm/min; ISO 527
2.90 GPa
421 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 87.0 MPa
12600 psi
2 mm/min; ISO 178
93.0 MPa
13500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
2 mm/min; ISO 178
2.70 GPa
392 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 7.50 J/cm
14.1 ft-lb/in
ASTM D256
1.50 J/cm
<br>@Temperature -30.0 °C
2.81 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
5.00 J/cm
<br>@Temperature 0.000 °C
9.37 ft-lb/in
<br>@Temperature 32.0 °F
ASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1A
12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
20.0 kJ/m²
<br>@Temperature 0.000 °C
9.52 ft-lb/in²
<br>@Temperature 32.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*4 sp=62mm; ISO 179/1eU
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
1.50 J/cm²
<br>@Temperature -30.0 °C
7.14 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 70.0 J
<br>@Temperature 23.0 °C
51.6 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
70.0 J
<br>@Temperature -20.0 °C
51.6 ft-lb
<br>@Temperature -4.00 °F
ASTM D3763
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
Taber Abrasion, mg/1000 Cycles 30
30
CS-17, 1 kg; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 69.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
80.0 µm/m-°C
<br>@Temperature -30.0 - 80.0 °C
44.4 µin/in-°F
<br>@Temperature -22.0 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 83.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
90.0 µm/m-°C
<br>@Temperature -30.0 - 80.0 °C
50.0 µin/in-°F
<br>@Temperature -22.0 - 176 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
120 °C
<br>@Thickness 3.20 mm
248 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
98.0 °C
<br>@Thickness 3.20 mm
208 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 131 °C
268 °F
Rate B/50; ASTM D1525
131 °C
268 °F
Rate B/50; ISO 306
133 °C
271 °F
Rate B/120; ISO 306