Polymer Property : Hardness, H358/30 = 105 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® BFL2000 PC
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific)
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East)
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® 1760T PBT+PC (Europe-Africa-Middle East)
XENOY 1760T is developed as a easy flow material, for applications such as doorhandles and mirror housings. It is a 11% glass reinforced material with excellent strength and dimensional stability.Th..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4810 PBT+PC
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4830 PBT+PC
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4850 PBT+PC
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4870HH PC+PET
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific)
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Hardness, H358/30 105 MPa
15200 psi
ISO 2039-1
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..