Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 100 - 200 °C
46.1 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 100 - 200 °C
46.1 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4810 PBT+PC
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS
LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East)
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific)
PPE+PS, HDT 125
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612  (Unverified Data**)
Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..
CTE, linear, Transverse to Flow 83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PX2060 PPE+PS
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..