Material Notes:
Medium viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Water Absorption 0.29 %
0.29 %
Saturation in water
Moisture Absorption at Equilibrium 0.12 %
0.12 %
Equilibrium at 50% RH
Water Absorption at Saturation 0.29 %
0.29 %
Melt Flow 8.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
8.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 100 MPa
14500 psi
Elongation at Break 3.5 %
3.5 %
Tensile Modulus 6.00 GPa
870 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Vicat Softening Point 145 °C
293 °F
Glass Transition Temp, Tg 148 °C
298 °F
UL RTI, Electrical 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL RTI, Mechanical with Impact 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL RTI, Mechanical without Impact 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 35 %
35 %
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 3.2

@Frequency 100 Hz
3.2

@Frequency 100 Hz
3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
Dielectric Strength 30.0 kV/mm
762 kV/in
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
0.0080

@Frequency 1e+6 Hz
0.0080

@Frequency 1e+6 Hz
Comparative Tracking Index 175 V
175 V