Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Mytex Polymers AN18KW-01 FK Polypropylene, Rubber modified Description: Rubber modified polypropylene produced for automotive interior applications using Mytex® Technology. Specifically designed to achieve ductile performance at cold temperatures during a.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Mytex Polymers AS78L(W)-GM-02 Polypropylene, Rubber modified, Compounded Description: AS78L(W)-GM-02 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties.Key Applications: Bumper fascias and all other exterior partsInform.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Mytex Polymers AS43L-01 Polypropylene, Rubber modified, Compounded Description: AS43L-01 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® MX 1002 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -20.0 °C |
23.8 ft-lb/in² @Temperature -4.00 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® HR 8234 - 10% Talc/Mineral Reinforced Polypropylene Copolymer, Very High Impact Strength & Flow 10% Mineral Reinforced, Very High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180 |
Polyram RamLloy B001 Nylon 6/Polyolefin Alloy, Impact Modified Nylon 6/Polyolefin alloy, reduction of water absorption, impact modified, for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® XT1627-BK2 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | partial; ISO 180/1A |
Domo 2500H Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |