Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer 25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Impact Test | 110 J | 81.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |