Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific) Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5.. |
|||
Vicat Softening Point | 133 °C | 271 °F | 50°C/h 50N; ISO 306 |
LATI LARIL 13 G/10 10% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Vicat Softening Point | 133 °C | 271 °F | ASTM 1525 B10 |
Metabolix Mirelâ„¢ P4001 Sheet Extrusion Grade Bioplastic Mirelâ„¢ P4001 is a general purpose, high melt strength material suitable for cast sheet extrusion. Mirelâ„¢ P4001 is designed for a wide range of sheet applications including gift cards, prom.. |
|||
Vicat Softening Point | 133 °C | 271 °F | 10N, 50°C/hr; ISO 306 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Vicat Softening Point | 133 °C @Load 1.02 kg |
271 °F @Load 2.25 lb |
Rate B (120°C/h); ASTM D1525 |
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color .. |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific) PPE+PS, HDT 125 |
|||
Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific) PPE+PS, HDT 125 |
|||
Vicat Softening Point | 133 °C | 271 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® T90 HT Polycarbonate + ABS Injection molding gradehigh heat resistanceVicat/B 120 = 135 °Cball indentation temperature = 125 °Ceasy flowsuitable for supporting life componentsPreprocessingMax. Water content |
|||
Vicat Softening Point | 133 °C | 271 °F | ASTM D1525 |
ExxonMobil EXACT™ 4053 Cast Plastomer Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Vicat Softening Point | 133 °C @Load 1.00 kg, Thickness 3.17 mm |
271 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ABSPC 9901B-50148 ABS/PC Blow Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 133 °C | 271 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ASA TW-18B1 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 133 °C @Load 1.00 kg, Thickness 3.17 mm |
271 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1527 |
Diamond Polymers DIAMALOY 530 PC/PBT Alloy, UV Stabilized/Weatherable Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 133 °C | 271 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
Vicat Softening Point | 133 °C | 271 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR6260 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 133 °C | 271 °F | 10N, 50°C/hr; ISO 306 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I.. |
|||
Vicat Softening Point | 133 °C | 271 °F | ASTM D1525 |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |