Polymer Property : Specific Gravity = 1.25 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable 2510-xx05D Polyvinyl Chloride Alloy (PVC Alloy)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Oxford Polymers OPX8320 Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads
Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers.
Specific Gravity 1.25 g/cc
1.25 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Specific Gravity 1.25 g/cc
1.25 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1-7332/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Loxim 315 01V0 Nylon 6
Information provided by Loxim Industries
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Loxim 315 02HB Nylon 6
Information provided by Loxim Industries
Specific Gravity 1.25 - 1.29 g/cc
1.25 - 1.29 g/cc
ASTM D 792
Karina 900D06/469-AT-IS Blue PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM 792
Multibase Multi-Flex® A 7727 HM Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D 792
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific)
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Specific Gravity 1.25 g/cc
1.25 g/cc
23°C; ASTM D792
Teknor Apex APEX® 2555-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Europe-Africa-Middle East)
NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting.
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA
NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance.
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Lubrizol Estane® S364D Thermoplastic Polyurethane
Type: Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
A. Schulman PAPERMATCH® H-3818 Specialty Masterbatch
DescriptionPAPERMATCH® H-3818 is a specialty masterbatch formulated to impart paper-like properties to polyethylene films. PAPERMATCH® H-3818 is a natural color, low opacity grade designed to pro..
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene
DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman.
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D 792
RTP Company RTP 2800 B-45A FR A Thermoplastic Polyolefin Elastomer (TEO); Flame Retardant - PBDE Free
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D 792
RTP Company RTP 2800 B-85A FR A UV Thermoplastic Polyolefin Elastomer (TEO) Flame Retardant - PBDE Free - UV Stabilized
Specific Gravity 1.25 g/cc
1.25 g/cc
23°C; ASTM D792
Teknor Apex Vidux® CV-1000-76 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- ExtrusionInformation provided by Teknor Apex Company
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Eastman Eastar EB062 Copolyester
Eastar Copolyester EB062 is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com..
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Eastman Provista ST Copolymer
Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation m..
Specific Gravity 1.25 g/cc
1.25 g/cc
Colorite Polymers Self Frosting™ 8511SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Colorite Polymers 7772 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D471; ISO 2781
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Specific Gravity 1.25 - 1.29 g/cc
1.25 - 1.29 g/cc
ASTM D-792
Axiall 11890 Wire & Cable Flexible PVC
High gloss, flame retardant jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
BLUESTAR LXS 314 G20 PPE-HIPS, 20% Glass Filled
Typical Applications: Water industrial partsInformation provided by Polymer Technology and Services, LLC (PTS).
Specific Gravity 1.25 g/cc
1.25 g/cc
silicone property; Arlon SQA-TMS-024
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Teknor Apex APEX® 3801-85 Polyvinyl Chloride, Flexible
Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex..
Specific Gravity 1.25 g/cc
1.25 g/cc
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Specific Gravity 1.25 g/cc
1.25 g/cc
Part B; TM R050-16
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
Specific Gravity 1.25 g/cc
1.25 g/cc
Zeon Chemicals Nipol® 9025 Polyblack Masterbatch
Recommended for use in extruded goods requiring medium-high solvent and oil resistance. Based on Nipol 35-5 with 75 phr of N660 black.Recommended for use in extruded goods requiring medium-high solv..