Mechanical Properties Metric English Comments
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Xenoy® X4810 PBT+PC
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Xenoy® X4830 PBT+PC
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer
25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East)
25 MFR LEXAN High Flow Ductile Copolymer
Impact Test 110 J
81.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized