Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® BFL2000 PC Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® 1760T PBT+PC (Europe-Africa-Middle East) XENOY 1760T is developed as a easy flow material, for applications such as doorhandles and mirror housings. It is a 11% glass reinforced material with excellent strength and dimensional stability.Th.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |