Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0055 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0055 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0045 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0045 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 5.5 g/10 min

@Load 5.00 kg,
Temperature 260 °C
5.5 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 39.0 MPa
5660 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 55 %
55 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 2.8 %
2.8 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.17 GPa
315 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 57.0 MPa
8270 psi
2.6 mm/min, 100 mm span; ASTM D790
61.0 MPa
8850 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.99 GPa
289 ksi
2.6 mm/min, 100 mm span; ASTM D790
2.06 GPa
299 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.32 J/cm
4.35 ft-lb/in
ASTM D256
Izod Impact, Unnotched 22.42 J/cm
42.00 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 32.0 J

@Temperature 23.0 °C
23.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 60.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 60.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 113 °C

@Thickness 3.20 mm
235 °F

@Thickness 0.126 in
unannealed; ASTM D648
116 °C

@Thickness 6.40 mm
241 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C

@Thickness 3.20 mm
207 °F

@Thickness 0.126 in
unannealed; ASTM D648
105 °C

@Thickness 6.40 mm
221 °F

@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 110 °C
230 °F
Rate B/50; ASTM D1525