Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 110 °C | 230 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Vicat Softening Point | 110 °C @Load 5.001 kg |
230 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 65 M10 PC/ABS-blend, Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Vicat Softening Point | 110 °C @Load 5.001 kg |
230 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5020 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 110 °C @Load 5.10 kg |
230 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® S 40EP3215 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Vicat Softening Point | 110 °C | 230 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND HI 18 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend, similar to KOBLEND HI 10 with improved impact resistance at low temperatures and better thermal properties. Main applicat.. |
|||
Vicat Softening Point | 110 °C | 230 °F | B |
Plastcom SLOVASTER® C FRU 2 PBT, flame retarder FeaturesPC with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other hole products. Application in engineer.. |
|||
Vicat Softening Point | 110 °C | 230 °F | ASTM D1525 |
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Vicat Softening Point | 110 °C @Load 5.00 kg |
230 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Vicat Softening Point | 110 °C | 230 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® C CM 206 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 110 °C | 230 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® C CM 206 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 110 °C | 230 °F | ISO 306 |
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and .. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Vicat Softening Point | 110 °C @Load 5.10 kg |
230 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Luran® S KR2866C ASA / PC Luran S KR2866C is a blend of ASA and PC with a reduced content of PC. It is characterized by a medium impact toughness and heat resistance.Good heat resistanceMedium impact strengthInformation prov.. |
|||
Vicat Softening Point | 110 °C | 230 °F | VST/B/50; ISO 306 |
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned) Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur.. |
|||
Vicat Softening Point | 110 °C | 230 °F | ASTM D1525 |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PX1185 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1185 is a special NORYL grade developed for extrusion of automotive trims. NORYL PX1185 offers high heat resistance and good impact performance. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
Vicat Softening Point | 110 °C | 230 °F | ASTM D1525 |
PlastxWorld CEVIAN®-V 420 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Vicat Softening Point | 110 °C | 230 °F | ASTM D1525 |
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer Zythane™ 4085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 110 °C @Thickness 2.00 mm |
230 °F @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D1525 |
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL FN150X PPE+PS Improved reliability and productivity. Thin wall capability. UL94 V-0/5VA rated. All data at 20% weight reduction and 0.250"" wall. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |