Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
cm³/10 min |
Polimeri Europa EDISTIR RC3 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-18 Special high impact, high gloss polystyrene grade. Suitable for injection molding in the appliances sector.. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238-62T |
Chevron Phillips 4518 LDPE Extrusion Coating Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Processability, Improved Drawdown, Good MVTR, Good Heat Seal, Kosher ApprovedApplications:Liquid Packaging, Cup Stock, Folding CartonData provided b.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® HXM TR-570 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This extra high molecular weight polyethylene is tailored for large containers with exhibit outstanding impact and creep resistance, excellent ESCR, and e.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman M30036-P Polyethylene
(discontinued **) M30036-P is an extrusion coating performance polymer suggested for applications requiring performance similar to LLDPE. Compared to low density coating resins, M30036-P offers superior heat seal st.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY NS5000 PC/ABS, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238G |
Hannam Chemical Hanalac 780 ABS, High Flow FDA Approved. High flow grade suitable for intricate or thin structures and low processing cycle time. Applications include TVs, radios, calculators, appliances, toys. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Adsylâ„¢ 5C30F Thermoplastic Olefin Resin Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature,.. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Melt Flow | 5.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 5.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5211R PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Melt Flow | 5.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |
|||
Melt Flow | 5.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® C513UV High Density Polyethylene, Blow Molding This extra high molecular weight, hexane copolymer is tailored for intermediate bulk container applications that require:Outstanding impact resistanceOutstanding ESCRExcellent processabilityUV stabi.. |
|||
Melt Flow | 5.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Melt Flow | 5.5 g/10 min | 5.5 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ FL 00623 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00623 is a good coextrusion partner in extrusion coating, blown and cast film. Excellent sealing material with a very low seal initiation temperature. Availability: Africa & .. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melt Flow | 5.5 - 7.5 g/10 min @Load 5.00 kg, Temperature 372 °C |
5.5 - 7.5 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
BASF Polystyrol® 576 H Impact Grade Polystyrene (Europe) Special tough to rigid grade with very good gloss for all types of housings.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Melt Flow | 5.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem Symbios 4102 Polypropylene Terpolymer Braskem Symbios 4102 is a medium melt flow rate terpolymer with a heat seal temperature below 120ºC on its treated face. It is designed for use as a heat sealing layer on bioriented films (BOPP) an.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont™ Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |