Polymer Property : CTE, linear, Parallel to Flow = 36.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific)
Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 193 PC
Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 194 PC
Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EM1210 PC
Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific)
Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EM3110 PC
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific)
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EM3110R PC
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific)
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 60.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 60.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PBT WM35 X
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES HiFill® POM CO GF5 CC 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 5% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES HiFill® PP GB30 30% Glass Beads Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and HomopolymerUL File Number: E157318Information provided by TP Composites,..
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES Plastiblend® ABS/PBT 1000
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled
Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl N1251 PPE+PS
ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES HiFill FR® PP CO E FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 64.8 µm/m-°C
36.0 µin/in-°F
ASTM D696
Techmer ES HiFill FR® PP CO FR HS
Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and CopolymerUL File Number: E157318Processing Method: Injection MoldingInformation provi..