Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 110 °C | 230 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Vicat Softening Point | 110 °C @Load 5.001 kg |
230 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5020 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 110 °C @Load 5.001 kg |
230 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5015 PD1 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 110 - 210 °C | 230 - 410 °F | Average value: 176 °C Grade Count:14 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Vicat Softening Point | 110 °C @Load 5.00 kg |
230 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Vicat Softening Point | 110 °C | 230 °F | ISO 306A |
Lucite International Diakon® ST35G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | <= 110 °C | <= 230 °F | |
Sibur ABS 0809M Molding Grade ABS Plastic Shock resistant with high thermal resistance for production of structural and decorative parts and articles of technical purpose. |
|||
Vicat Softening Point | 110 °C | 230 °F | Unannealed; ISO R-306 |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 110 °C | 230 °F | VST/B/50; ISO 306 |
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned) Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur.. |
|||
Vicat Softening Point | 110 °C | 230 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 110 °C | 230 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 190A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 110 °C | 230 °F | ASTM D1525 |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East) NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade. |
|||
Vicat Softening Point | 110 °C @Load 1.02 kg |
230 °F @Load 2.25 lb |
Rate B (120°C/h); ASTM D1525 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Vicat Softening Point | 110 °C | 230 °F | |
Covestro Bayblend® T 44 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 45 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Vicat Softening Point | 110 °C | 230 °F | 49 N; ISO 306 |
A.D. Compound Adene NCWA Homopolymer 60% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 110 °C @Load 5.001 kg |
230 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF8020 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 110 °C @Thickness 2.00 mm |
230 °F @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D1525 |
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Vicat Softening Point | 110 °C | 230 °F | |
Ineos ABS NOVODUR® P2T ABS, Injection Grade
(discontinued **) Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g.. |
|||
Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL FN150X PPE+PS Improved reliability and productivity. Thin wall capability. UL94 V-0/5VA rated. All data at 20% weight reduction and 0.250"" wall. |
|||
Vicat Softening Point | 110 °C | 230 °F | 50B; ISO 306 |
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers |