Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C

@Thickness 6.40 mm
241 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Deflection Temperature at 0.46 MPa (66 psi) 116 °C

@Thickness 6.40 mm
241 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.