Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE UMERIT 2525F Metallocene LLDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer UBE
Trade Name UMERIT
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UMERIT 2525F Metallocene LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical properties by being able to acquire any targeted molecular structures. Specific Notes for this Grade: UMERIT® 2525F offers various excellent properties: Excellent heat resistance, Well-balanced of impact strength and stiffness, Low taste/odor, Good film appearance : reduced fish-eyes and lower Haze/Higher GlossInformation provided by UBE.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 1000 hour
1000 hour
F50; ASTM D1693
Melt Flow 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 715 %
715 %
ASTM D638
Tensile Modulus 0.330 GPa
47.9 ksi
Bending Modulus; ASTM D790
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
UBE method
Vicat Softening Point 113 °C
235 °F
ASTM D1525