Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Plaskolite Duraplex® 100% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR3020 ASA Low-gloss ASA for profile and capstock applications |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min |
Polimeri Europa SINKRAL B620 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-25-20 High impact injection moulding grade. Its` excellent balance of mechanical properties (toughness -.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min |
Polimeri Europa SINKRAL B733/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,095-04-35-15 Very high impact resistant grade for sheet extrusion with good processability and high thermal sta.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Flint Hills P4C6B-134A Polypropylene Homopolymer Features: Excellent processability, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Cutlery, Consumer Products, Cosmetic.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Flint Hills P4G4K-038 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and clarified.Applications: Injection molding: high clarity, housewares, and syringes, for EO sterilization.Former Huntsma.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6 PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | conditioned |
Ineos ABS Triax® KU2-3154 ABS + Nylon 6 Mineral reinforced, easy flowing, reduced moisture absorption, very low warpage, injection molding, pellets.,Property data per ISO test methods. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 type 1 A |
Solvay TECHNYL® C 230 PA6, Conditioned Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: This grade has improved impact strength and higher flexibili.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527-2/50 |
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 100mm/min; ISO 527-2 |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Teknor Apex Sinpolene TPP1010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Housings Forms: Pellets Processing Method: Injection Mol.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Teknor Apex Sinpolene TPP1020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 20% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527-1/-2 |
Unitika EX-1030 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527-2 |
Denka MALECCA K-200 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Entec Hypro™ PP-HP20NS Homopolymer, 20 Melt Flow, Nucleated, Anti-stat This product is intended for general purpose injection molding applications such as cutlery, caps and closures, and thin-wall containers.Information provided by Entec |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow, Nucleated, Anti-stat This product is intended for thin-wall injection molding applications such as caps and closures, food containers and consumer products that require high stiffness.Information provided by Entec |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min |
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334G10M20CL Glass/Mineral Reinforced Coupled |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 23; ISO 527 |
BASF Ultramid® 8200 HS PA 6 (Conditioned) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Cheng Yu Plastic A779 Lubrication ABS |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |