Lehmann & Voss LUVOCOM® 1850-7692 PBT, with glass spheres and PTFE

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), PTFE Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1850-7692 PBT, with glass spheres and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding elements and other duty parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
Mechanical Properties Metric English Comments
Tensile Stress 35.0 MPa
5080 psi
Elongation at Yield 3.0 %
3.0 %
4.0 %
4.0 %
flexural
Modulus of Elasticity 3.00 GPa
435 ksi
Flexural Strength 50.0 MPa
7250 psi
Flexural Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Coefficient of Friction, Dynamic 0.20
0.20
Coefficient of Friction, Static 0.15
0.15
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
150 °C
302 °F
short term
Vicat Softening Point 205 °C
401 °F
DIN ISO 306
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
mass temp
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Zone 1 240 - 260 °C
464 - 500 °F
Zone 2 260 - 280 °C
500 - 536 °F
Zone 3 250 - 270 °C
482 - 518 °F
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Vacuum Dryer
120 °C

@Time 14400 - 21600 sec
248 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (white)