Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
NYCOA 1637 PA 6
plasticized and heat stabilized extrusion grade for the wire jacketing industry to 7,000+ fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
Processing Temperature 250 °C
482 °F
NYCOA 27/300I Glass Filled Nylon 6
30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc.
Processing Temperature 250 °C
482 °F
NYCOA 446 PA 6
UL-94 V-2 rated for flammability extrusion grade for rod, sheet and filmInformation provided by NYCOA, Inc.
Processing Temperature <= 250 °C
<= 482 °F
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class ..
Processing Temperature 250 °C
482 °F
mass temp
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Processing Temperature 250 °C
482 °F
mass temp
Lehmann & Voss LUVOCOM® 1850-8098 PBT, with glass fiber, thermally conductive modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.High dimensionally stable precision parts, even at elevated temperatures an..
Processing Temperature 250 °C
482 °F
mass temp
Lehmann & Voss LUVOCOM® 6-7433 Polyamide 12, with carbon fiber, hydrolysis resistant
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
Processing Temperature 250 °C
482 °F
mass temp
Lehmann & Voss LUVOCOM® 6-7833 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh..
Processing Temperature 250 °C
482 °F
mass temp
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab..
Processing Temperature 250 - 260 °C
482 - 500 °F
CF
UBE 1022FDX23 Nylon 6 Homopolymer Film
Specialties: High slip typeProcessing: Water cooling processTypical applications: small pouch & generalInformation provided by UBE.
Processing Temperature <= 250 °C
<= 482 °F
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Processing Temperature 250 - 270 °C
482 - 518 °F
Eurotec® Tecodur® PB70 GB20 NL PBT, 20% glass bead reinforced, natural
Information provided by Eurotec®
Processing Temperature 250 - 270 °C
482 - 518 °F
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural
Information provided by Eurotec®
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 1600A PBT, Unfilled
Celanex 1600A is a high molecular weight grade of unreinforced polybutylene terephthalate used in both extrusion and injection molding applications.Information provided by Celanese
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 2401 MT PBT, Medical Technology
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 3100-2 PBT, 7.5% Glass Reinforced
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.Information ..
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 3200-2FC PBT, 15% Glass Reinforced
Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3..
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 3309HRT PBT, 30% Glass Reinforced
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celanese
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 3316HR PBT, 30% Glass Reinforced
Celanex 3316HR is a flame retarded, hydrolysis resistant, 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability.Information..
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 4306UV PBT, 30% Glass Reinforced
Celanex 4306UV is a 30% glass reinforced, toughened, low warpage, UV stable thermoplastic polyester.Information provided by Celanese
Processing Temperature 250 - 300 °C
482 - 572 °F
Resin Temperature
Asahi Kasei Xyron® X0722 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
Processing Temperature 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
Processing Temperature 250 - 265 °C
482 - 509 °F
hot runner
Celanese CELANEX 6500 PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.Information provided by Celanese
Processing Temperature 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture)
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
Processing Temperature 250 - 290 °C
482 - 554 °F
Zhejiang Juner PC-A1-7 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
Processing Temperature 250 - 270 °C
482 - 518 °F
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural
Information provided by Eurotec®
Processing Temperature 250 - 260 °C
482 - 500 °F
hot runner
Celanese CELANEX 7716 PBT, 35% Mineral / Glass Reinforced
Celanex 7716 is a 35% glass/mineral reinforced, non exuding, flame retarded polybutylene terephthlate which has and excellent balance of mechanical properties and processability. Celanex 7716 is wel..
Processing Temperature 250 - 270 °C
482 - 518 °F
E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM
Super ToughnessInformation provided by E-Polymers Co. Ltd.