Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 35.0 MPa | 5080 psi | |
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | |
Lehmann & Voss LUVOCOM® 1850-7692 PBT, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | at Break; ISO 527 |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | at Break; ISO 527 |
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse .. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | at Break; ISO 527 |
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene EX5 is a high density polyethylene with 1-Butene as co monomer.Applications: film extrusion, counter bag, carrier bag, wrapping filmsInformation provided by Iran Petrochemical Commercial Co. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | ISO R527 |
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene Moplen Z 30S is a high melt flow homopolymer for the production of low denier BCF, CF, and staple fibers at medium to high spinning speeds. Moplen Z30S offers a high homogeneity, stable extrusion a.. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | at Break; ISO 527 |
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending .. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | ISO R527 |
Iran Petrochemical (PCC) S 28 F Polypropylene Film Biaxially oriented poly propylene films suitable for metallization Applications: cosmetics , food stuffs , lamination and other flexible films.Information provided by Iran Petrochemical Commercial C.. |
|||
Tensile Stress | 35.0 MPa | 5080 psi | ISO R527 |
Iran Petrochemical (PCC) S 30 G Polypropylene The grade has combined excellent process ability with high stiffness.Applications: bags, mats, packing twines and ropes, drinking beakers packaging for dairy products.Information provided by Iran Pe.. |
|||
Tensile Stress | 35.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
5080 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |
|||
Tensile Stress | 35.0 MPa @Strain 50.0 % |
5080 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |