Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 230 - 260 °C | 446 - 500 °F | hopper |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/CF/15/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7854 PBT, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7952 PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8197 PBT, lubricant modified, easy flowing, demolding aid Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8282 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7557 PBT, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour, self-lubricating, for highest tribologic needs.Low warpag.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 230 - 260 °C | 446 - 500 °F | |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Zone 1 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide 6 80E7 PA6, Injection Molded Staramide 6 80E7 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E7)Information provided by Eurostar. |
|||
Zone 1 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide PF00A PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00A is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide PF00AE PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AE is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |