Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 240 °C | 464 °F | Die |
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6 Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | hopper |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7315 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7692/BK PBT, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7942 PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8197 PBT, lubricant modified, easy flowing, demolding aid Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | |
Lehmann & Voss LUVOCOM® 7-0755 Polyamide 610, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.Improved friction and wear behaviou.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 290 °C | 464 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Zone 1 | 240 - 290 °C | 464 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Star L PA6 30V D51 PA6, Glass Filled, Injection Molding Star L PA6 30V D51 is a PTFE Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX06004 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta.. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded Starflam PX06091 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX07037 PA6, Flame Retardant, Injection Molded Starflam PX07037 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (IR laser marking grade)Information provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PK00032E PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0032E is a Halogen Free Red Phosphorous Free Flame Retardant Mineral Filled Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 °C | 464 °F | Feeding zone |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |